Cost-effective Manufacturing of Large-Volume Components

Tool cavity of tool steel, made with SLM and filled with grey cast iron. (Source: Fraunhofer ILT)

Tool cavity of tool steel, made with SLM and filled with grey cast iron. (Source: Fraunhofer ILT)

In the past, selective laser melting (SLM) technology has been cost effective only for manufacturing components with relatively small volumes. In an innovative breakthrough that combines SLM with casting, now the Fraunhofer Institute for Laser Technology ILT has developed a cost-effective method for manufacturing solid, large-volume components using SLM. For the first time at EuroMold 2014, experts presented tool inserts with conformal cooling channels that were made using the combined method.
Injection molding is used to make the majority of plastic components. With additive manufacturing techniques such as SLM, it is possible to integrate complex conformal cooling channels into the tool inserts required for injection molding. These channels allow the tool mold to be heated up during the injection process, and the melt to cool down quickly and evenly – resulting in rapid, distortion-free manufacturing. However, the manufacture of large-volume tool inserts using SLM is very cost-intensive, because the main production costs are volume-dependent.
To tackle this problem, scientists from Fraunhofer ILT have teamed up with the Foundry Institute at RWTH Aachen University and partners from industry in a bid to combine SLM and casting methods. In the “GenCast” pro­ject, which is funded by the German Federal Ministry of Education and Research as part of the Central Innovation Program SME (or “ZIM” in German), the project partners have worked together to build up the requisite process understanding and developed the process chain for the combined method.
The idea behind combining the two methods is to manufacture the shell of the tool insert from hot work steels (1.2343 or 1.2709) using SLM. During this process, cooling channels with complex geometries are still integrated in the exact places where they are needed to heat or cool the component. The shell built up using this technique serves as a casting mold, which is rapidly and cost-effectively filled with gray cast iron (e. g. GJL-200) or highly thermal conductive copper in a subsequent casting process. This cuts production times by up to eighty per cent compared to components made using SLM alone. The bigger a component is, the more the advantages of this combined method come into play. It can be used cost-effectively from part sizes of only half a liter upward. (Source: Laser Technik Journal 1 / 2015)

Links: Fraunhofer ILT, Aachen